Sample and materials
- Sample: Al-wt%Cu alloy
- Dimension: 1.4mm in diameter, 6.5mm in length
Experiment and characterisation
- Heat treatment: 15min annealing at 630°C in a muffle furnace, air cooling to room temperature
- X-ray imaging equipment: ZEISS Xradia 520 Versa X-ray microscope with LabDCT pro module
- Absorption contrast tomography scan: 80kV-7W, 4X detector, 1601 projections, 1.84 µm voxel size
- Diffraction contrast tomography scan: 110kV-10W, flat panel detector, helical phyllotaxis scanning scheme, 2900 projections
Data
- Number of datasets: 11
- Format: .dream3d
- Naming: t0 - initial state, t10 - after the 10th annealing treatment